Microstructure and 3-D effects in fretting fatigue of Ti alloys and Ni-base superalloysReportar como inadecuado


Microstructure and 3-D effects in fretting fatigue of Ti alloys and Ni-base superalloys


Microstructure and 3-D effects in fretting fatigue of Ti alloys and Ni-base superalloys - Descarga este documento en PDF. Documentación en PDF para descargar gratis. Disponible también para leer online.