Reference: King, A, Johnson, G, Engelberg, D et al., (2008). Observations of intergranular stress corrosion cracking in a grain-mapped polycrystal. Science (New York, N.Y.), 321 (5887), 382-385.Citable link to this page:

 

Observations of intergranular stress corrosion cracking in a grain-mapped polycrystal.

Abstract: Nondestructive three-dimensional mapping of grain shape, crystallographic orientation, and grain boundary geometry by diffraction contrast tomography (DCT) provides opportunities for the study of the interaction between intergranular stress corrosion cracking and microstructure. A stress corrosion crack was grown through a volume of sensitized austenitic stainless steel mapped with DCT and observed in situ by synchrotron tomography. Several sensitization-resistant crack-bridging boundaries were identified, and although they have special geometric properties, they are not the twin variant boundaries usually maximized during grain boundary engineering.

Publication status:Published

Bibliographic Details

Journal: Science (New York, N.Y.)see more from them

Issue Date: 2008-7

pages:382-385Identifiers

Urn: uuid:29281ecc-84be-4563-94c4-07c21acbabb0

Source identifier: 177388

Eissn: 1095-9203

Doi: https://doi.org/10.1126/science.1156211

Issn: 0036-8075 Item Description

Type: Journal article;

Language: eng Tiny URL: pubs:177388

Relationships





Autor: King, A - - - Johnson, G - - - Engelberg, D - - - Ludwig, W - - - Marrow, J - - - - Bibliographic Details Journal: Science New Yo

Fuente: https://ora.ox.ac.uk/objects/uuid:29281ecc-84be-4563-94c4-07c21acbabb0



DESCARGAR PDF




Documentos relacionados